Login to supply and review
project info, drawings, price quotes, etc. (Quote
form) |
|
|
|
|
 |
|
|
EA Magnetics
|

EA Magnetics - Injection Molded Neodymium Magnet Information

 |
|
|
Injection Molded Neodymium
& Hard Ferrite
MAGNETIC PROPERTIES

Viewing: Magnetic Properties
of Injection Molded Neodymium
See also:
Physical Properties of Injection Molded Neodymium
See also:
Injection Molded Neodymium Demagnetization Chart
Download:
EAM-InjMoldedNeoFerrite-MagPhysProps.pdf - 350 Kb |
|
Product
Name |
Anisotropic Magnet |
Isotropic Magnet |
Residual
flux
density |
Coercive force |
Maximum
energy
product |
Residual
flux
density |
Coercive force |
Maximum
energy
product |
|
Br |
bHc |
iHc |
(BH) max. |
Br |
bHc |
iHc |
(BH) max. |
|
(G) |
(Oe) |
(Oe) |
(MGOe) |
(G) |
(Oe) |
(Oe) |
(MGOe) |
|
Hard Ferrite / NYLON 6 |
| EAM 9500 |
1000 |
950 |
1900 |
0.2 |
650 |
650 |
2000 |
0.1 |
| 140 |
2400 |
2200 |
2900 |
1.4 |
1250 |
1100 |
2900 |
0.3 |
| 160 |
2600 |
2250 |
2850 |
1.6 |
1370 |
1140 |
2800 |
0.4 |
| 170 |
2780 |
2350 |
2800 |
1.8 |
1450 |
1200 |
2800 |
0.5 |
| 190 |
2870 |
2350 |
2700 |
2.0 |
1480 |
1250 |
2700 |
0.5 |
| 200 |
3000 |
2400 |
2800 |
2.2 |
1530 |
1300 |
2800 |
0.6 |
|
Hard Ferrite / Nylon 12 |
| 062 |
1550 |
1400 |
2000 |
0.6 |
1050 |
1000 |
2000 |
0.2 |
| 132 |
2340 |
2200 |
3300 |
1.4 |
1200 |
1150 |
3250 |
0.3 |
| 152 |
2570 |
2350 |
3300 |
1.6 |
1320 |
1200 |
3250 |
0.4 |
| 172 |
2730 |
2400 |
2900 |
1.8 |
1400 |
1250 |
2850 |
0.4 |
| 192 |
2860 |
2400 |
2900 |
2.0 |
1460 |
1250 |
2850 |
0.5 |
| 202 |
2930 |
2500 |
2900 |
2.1 |
1500 |
1300 |
2850 |
0.6 |
|
Hard Ferrite / PPS |
| 134 |
2350 |
2200 |
2850 |
1.4 |
1200 |
1150 |
2800 |
0.3 |
| 164 |
2640 |
2250 |
2800 |
1.7 |
1380 |
1200 |
2750 |
0.4 |
|
Nd-Fe-B
/ Nylon 12 |
| 362 |
— |
— |
— |
— |
4000 |
3450 |
7900 |
3.3 |
| 392 |
— |
— |
— |
— |
5000 |
3900 |
8000 |
5.0 |
| 502 |
— |
— |
— |
— |
5700 |
4200 |
7500 |
6.0 |
| 602 |
— |
— |
— |
— |
6100 |
4250 |
7500 |
7.0 |

|
Product
Name |
Saturated flux
density |
A.C. initial permeability

µiac |
Relative loss factor

tan / µiac |
Volume
Resistivity |
|
Bs |
100KHz |
1MHz |
100KHz |
1MHz |
|
|
(G) |
— |
— |
— |
— |
Ω • m |
|
Soft Ferrite / NYLON 6 |
| 410 |
3200 |
11.5 |
11.5 |
4.4 X 10-3 |
1.0 X 10-3 |
103 |
| 425 |
2450 |
15.0 |
15.0 |
2.8 X 10-3 |
8.0 X 10-3 |
107 |
|
Soft Ferrite / NYLON 12 |
| 422 |
3100 |
10.4 |
10.4 |
6.4 X 10-3 |
1.4 X 10-3 |
103 |
|
Soft Ferrite / Polyotefine |
| 430 E |
3050 |
10.1 |
10.1 |
5.6 X 10-3 |
1.3 X 10-3 |
103 |
|
Soft
Ferrite / PPS |
| 456 S |
650 |
2.9 |
2.9 |
7.5 X 10-3 |
1.1 X 10-3 |
1011 |
| 465 N |
2470 |
16.0 |
16.0 |
2.7 X 10-3 |
1.5 X 10-3 |
108 |
| • |
Conversion Formula (CGS unit SI unit) -
1G=10-4T 10e=80A/m 1MG0e=8kJ/m3 |
| • |
The above tables are based on reliable sources
for reference only. |
| • |
Users are advised to utilize them only after
study of all relevant data. |
|
 |
|